Sliding wear behaviour of HVOF and HVAF sprayed Cr3C2-based coatings

Academic Article
Publication Date:
2017
Short description:
Sliding wear behaviour of HVOF and HVAF sprayed Cr3C2-based coatings / Matikainen, V.; Bolelli, G.; Koivuluoto, H.; Sassatelli, P.; Lusvarghi, L.; Vuoristo, P.. - In: WEAR. - ISSN 0043-1648. - 388-389:(2017), pp. 57-71. [10.1016/j.wear.2017.04.001]
abstract:
Thermally sprayed tungsten carbide (WC) and chromium carbide (Cr3C2) based hard metal coatings are commonly applied on component surfaces as corrosion and wear resistant layers. Typically, WC-Co/Ni with optional Cr addition and Cr3C2-25NiCr powders are sprayed with high velocity oxy-fuel (HVOF) or high velocity air-fuel (HVAF) processes. Due to the poor oxidation resistance of the WC particles, Cr3C2-25NiCr composition is typically selected for high temperature environments, up to 800–900 °C. In this study, two distinct Cr3C2-based compositions of Cr3C2-50NiCrMoNb and Cr3C2-37WC-18NiCoCr were selected as interesting alternatives to conventional Cr3C2-25NiCr. Sliding wear behavior of the coatings sprayed with HVOF and HVAF processes were tested with a ball-on-disk configuration against an Al2O3ball at room temperature and at 700 °C. It was found that both alternative materials had comparable coefficients of friction with the Cr3C2-25NiCr coatings. The Cr3C2-37WC-18NiCoCr coatings provided improved wear resistance at room temperature conditions, but at 700 °C the wear rate was increased to the level of the Cr3C2-50NiCrMoNb coatings. Cr3C2-25NiCr coatings experienced the lowest wear rates at elevated temperatures, which was even lower than at room temperature.
Iris type:
Articolo su rivista
Keywords:
Cr3C2; HVAF; HVOF; Sliding wear; Thermal spray coatings; Condensed Matter Physics; Mechanics of Materials; Surfaces and Interfaces; Surfaces, Coatings and Films; Materials Chemistry2506 Metals and Alloys
List of contributors:
Matikainen, V.; Bolelli, G.; Koivuluoto, H.; Sassatelli, P.; Lusvarghi, L.; Vuoristo, P.
Authors of the University:
BOLELLI Giovanni
LUSVARGHI Luca
Handle:
https://iris.unimore.it/handle/11380/1154586
Full Text:
https://iris.unimore.it//retrieve/handle/11380/1154586/399077/Sliding%20wear%20behaviour%20of%20HVOF%20and%20HVAF_ACCEPTED_MANUSCRIPT.pdf
Published in:
WEAR
Journal
  • Use of cookies

Powered by VIVO | Designed by Cineca | 26.4.5.0